Catalog No. | CY2429 |
---|---|
Size | 5×5 mm, 5×10 mm, 10×10 mm, 20×20 mm |
Purity | 99.995 % |
Orientation | (100), (110), (111), +/- 0.5 degree |
Growth Method | Vernue (flame) method |
A variety size of strontium titanate crystal substrates can be offered by Stanford Advanced Materials (SAM). We have a professional sales team to offer a fast response within 24 hours and warm service.
Strontium titanate crystal substrate has its lattice parameters match most materials with a Perovskite crystal structure, and therefore it is a popular crystal substrate for epitaxial growth of many oxide thin films. It is commonly used as a substrate material for superconductor thin films, because Strontium Titanate (SrTiO3) and Y-Ba-Cu-O system (a = 3.89 A) have similar values in the lattice constant.
Crystal structure |
Cubic, Perovskite |
Molar mass (g/mol) |
183.49 |
Growth method |
Vernue (flame) method |
Purity (%) |
>99.9 |
Density (g/cm3) |
5.11 |
Hardness |
6-6.5 Mohs |
Chemical stability |
Insoluble in water |
Sizes |
5×5 mm, 5×10 mm, 10×10 mm, 20×20 mm, or special sizes and orientations are available upon request |
Thickness |
0.5mm, 1.0mm |
Polishing |
Single side polished (SSP) or double side polished (DSP), Epi-ready surface Ra < 0.5 nm |
Orientation |
(100), (110), (111) +/-0.5 degree |
Package |
Packed in class 100 grade plastic bag in class 1000 cleanroom |
Strontium titanate crystal substrate has been used widely for special optical windows and as high quality sputtering target. It is also suitable for different film growth technologies such as Magnet Sputtering, Pulsed Laser Deposition (PLD), Vapourization, MOCVD, CVD, and laser MBE, etc. Films made by these materials and technologies on SrTiO3 substrate have excellent performance, for instance Tc>90K, Jc> = 106A/cm2.