(949) 407-8904 Mon - Fri 08:00 - 17:00 23661 Birtcher Dr., Lake Forest, California, USA
(949) 407-8904 Mon - Fri 08:00 - 17:00 23661 Birtcher Dr., Lake Forest, California, USA

TS1385 Nickel-based Superalloy Powder

Catalog No. TS1385
Material Nickel Alloy Powder
Appearance Dark Gray Powder
Particle Size 20-125 um, or as request

Stanford Advanced Materials (SAM) supplies high quality Nickel-based Superalloy Powder with competitive price.




Description

Nickel-based Superalloy Powder Description

Nickel metal has a silvery-white luster and a slight golden color. Nickel is a transition metal, hard and ductile. Pure nickel, powdered to maximize the reactive surface area, shows a significant chemical activity, but larger pieces are slow to react with air under standard conditions because an oxide layer forms on the surface and prevents further corrosion (passivation). Nickel-based Superalloy Powder includes Ni-Cr, Ni-Mn and other stainless powder. It has outstanding high temperature strength and oxidation resistance.

nickel-based super alloy powder

Nickel-based Superalloy Powder Specifications

Item No.

Materials

Chemical Composition (wt%)

Particle Size

Coating process

C

Cr

Si

W

Fe

Mo

Ni

Co

Mn

Nb

Ni28-01S

NiCr20

0.2Max

20

1

0.5Max

Bal

0.5Max

53-20μm

HVOF

Ni28-02S

NiCr50

1.0Max

50

1

0.5Max

Bal

0.5Max

106-45μm

Plasma Spraing

Ni28-03S

Ni625

0.1

20.0-23.0

/

/

5

8.0-10.0

Bal

/

/

3.15-4.15

53-20μm

HVOF

Ni28-04S

Ni-C

0.1

16.5

0.9

4.5

5.5

17

Bal

2.0Max

0.9

53-20μm

HVOF

Ni28-05S

Ni-SuperC

0.05Max

23

18

Bal

53-20μm

HVOF

Ni28-06S

Ni276

0.01Max

15.5

0.03

4

16

Bal

2.5Max

1

53-20μm

HVOF

Ni28-07S

Mn400

0.15Max

1.25

1.5

Ti:2.0

Bal

3.5

Cu:28.0

53-20μm

HVOF

Nickel-based Superalloy Powder Applications

With excellent overall performance, resistance corrosion, oxidation, heat resistance and low-stress abrasion and adhesive wear resistance, Nickel-based Superalloy Powder can be applied to a various process including:
-Oxyacetylene spraying or overlaying
-HVOF/HAFA spraying
-Plasma transferred arc (PTA) overlaying
-Plasma spraying
-Laser overlaying
-Induction melting overlaying
-Centrifugal casting
-3D printing and powder metallurgical processing

Nickel-based Superalloy Powder Packing

25KG per drum or as required
Our Nickel-based Superalloy Powder is clearly tagged and labeled externally to ensure efficient identification and quality control. Great care is taken to avoid any damage which might be caused during storage or transportation.

Submit your review
1
2
3
4
5
Submit
     
Cancel

Create your own review

Nickel-based Superalloy Powder
Average rating:  
 1 reviews
by Ryan Morrow on Nickel-based Superalloy Powder

I highly recommend SAM's products especially because they offer the powder of good quality. Will buy again.