Target magnetic field The cathode operating voltage of magnetron sputtering decreases as the target surface magnetic field increases, and also decreases as the sputtering etch groove of the target surface deepens. The sputtering current increases as the sputter etch bath of the target surface deepens because the sputter etched surface of the target gets closer...Continue Reading